Bottom Surface quality improvement in ALCATEL DRIE process
Pradeep Dixit
2006-02-24
Dear All,

I am facing problem in getting smmoth bottom surface in DRIE process by
ALCATEL machine.
Process parameters are - SF6- 300, C4F8- 150, etch/pass - 7/2, Coil power -
1800 W, platen - 80 W, temperature - 10C.

Surface obtained after etching (even after 5 min etch) is rough.

Can any one advice me anything to make the surface smooth or to improve the
surface quality after etching process. Can any one suggest some suitable
recipe for getting smooth surface? I will not mind if this new recipe affect
the etch rate. My priority is to get as smooth surface as possible. Will
reducing the C4F8 will help ?

--
Thanks,
Pradeep Dixit
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing