All,

What is the optimum bonding temperature for quartz bonds? I have tried 1100
degree C for making microfluidic channels. However, I observe leakage of
current between two closely lying channels over time. I suspect the bonding
between the substrates in failing.

Has anyone had a similar experience? Any suggestions on this matter would be
appreciated.

Thanks,
Rajiv.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Mentor Graphics Corporation
University Wafer