MEMSnet Home: MEMS-Talk: Hydrophillic PDMS
Hydrophillic PDMS
2006-06-29
g.balsubra manian
Improving particle's microwave energy absorption under airflow condition/entrainment process
2006-06-29
wahid YEMI.
Hydrophillic PDMS
g.balsubra manian
2006-06-29
Hi Guys.,

I am working in PDMS microchannels. I want to convert
the PDMS surface to hydrophillic.  I want to use
sodium silicate solution for converting the
hydrophobic surface to hydrophillic rather than using
Plasmma Oxygen treatment.

Anyone knows what is the method for treatment of
sodium silicate??.  I am not able to get required data
for the above one.

Thanks

Bala.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Nano-Master, Inc.
Harrick Plasma, Inc.