Blue color on some parts
amron gary
2006-07-10
Hello all,

We work in decorative hard coatings on 3D objects. I
am having two problems:

1. I am seeing some blue color on some portions of the
parts whereas rest of the parts on the turntable look
fine. Any suggestions???

2. Also, some of the parts even do not get any PVD
coating whereas other parts on the same turntable get
PVD coating fine. Any suggestions to solve these two
problems in my Arc Evaporation PVD system. Thanks in
advance.

Gary
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation