2006-09-04
[email protected]
dissolving cured epoxy glue
ssood
2006-09-05
Miller Stephenson makes a product- MS-111 epoxy stripper that works pretty
good to remove cured epoxies.
Not sure as to what effect it might have on your sensors though, as the
sample would need to be soaked in the stripper for some time.

Sumant Sood
Belford Research Inc.

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Mohammad Najmzadeh
Sent: Monday, September 04, 2006 3:53 PM
To: [email protected]
Subject: [mems-talk] dissolving cured epoxy glue

Hello,

I have attached some silicon sensors to an aluminium setup with epoxy glue
and now I want to disconnect them.

I am looking for a way to dissolve this cured epoxy glue.

Heating of it for 3 hours on a hot plate with 200-300 degree C was one
option to dissociate that glue but that was not successful.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation