MEMSnet Home: MEMS-Talk: Nickel deposition technique!
Nickel deposition technique!
2006-10-16
madhav rao
2006-10-16
g.balsubra manian
2006-10-16
David Nemeth
2006-10-18
madhav rao
Nickel deposition technique!
g.balsubra manian
2006-10-16
For good thickness., you need to electroplate. For
good control over thickness (less thickness),u can do
either sputtering or evaporation.

For electroplating.,Ti or Cr Seed layer should be
either sputtered or evaporated.

Sputtering by e-beam should be better than thermal
evaporation as temp can be higher in the evaporation.

Regards

Bala


--- madhav rao  wrote:

> Hi all,
>       I am planning to deposit Nickel on silicon
> wafer. However im using PMMA patterning. Hence i
> need
> to do liftoff. Can u suggest a simpler way of
> depositing nickel such as sputtering or evaporation
> or
> electroplating. Let me know!!
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
Mentor Graphics Corporation
MEMS Technology Review