A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: etch through hole on pyrex glass
etch through hole on pyrex glass
2006-12-12
Hui Ju
2006-12-12
Shay Kaplan
Glas Frit Bonding
2006-12-13
Erik Jung
2006-12-13
Gareth Jenkins
2006-12-13
Shay Kaplan
2006-12-13
Anil Agiral
2006-12-14
Pradeep Dixit
etch through hole on pyrex glass
Shay Kaplan
2006-12-12
It depends on the aspect ration you need. In both available technologies -
ultrasonic drilling and sandblasting, you will get ~45 deg or better angles.
You can DRIE but it will contaminate the system and take many hours to open.

Shay

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Hui Ju
Sent: Tuesday, December 12, 2006 3:17 AM
To: [email protected]
Subject: [mems-talk] etch through hole on pyrex glass

Dear Everybody,
Hello!
Does anyone know how to make holes with a diameter of about 200 microns on
pyrex glass (7740, thickness of 200 microns)? I
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMStaff Inc.