Gareth Jenkins
2007-01-19
What do you mean by no success - poor quality or something else? The
type of glass is also relevant. I have had good results with 2% conc. HF
+ 2% conc. HNO3 when using soda-lime glass. I have never tried it on
quartz though, but I would not expect it to etch at a similar rate.


Barbara Cortese wrote:
> Hi to all
>
> I'm etching glass and quartz by a wet etching solution of BHF, but my recipe
isn't too good. I've tried differrent solutions with no success. Has anyone a
good recipe to suggest me?(not just saying BHF 6:1! but the effective
quantities!).
>
>

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing