MEMSnet Home: MEMS-Talk: pH adjusting of NiP plating bath
pH adjusting of NiP plating bath
2007-02-08
Zhang Xiao Qiang
pH adjusting of NiP plating bath
Zhang Xiao Qiang
2007-02-08
Hi,

I am trying to get NiP pattern with plating. Anyone have relevant
experience? Some papers reported that the bath's pH value should be
around 3-5. The as obtained bathes have pH near 0-1wether you use H3PO4
or NaH2PO3. The normal way to get this value is add NaOH but I found it
is quite hard to handle it since NaOH reacts with Ni2SO4 and the product
is not easy-solving in water?

Any comments and suggestions are appreciated.

Thanks!

Zhang
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.