Hi all

    I need to deposite 0.3um LP Si3N4 on <100> Si wafer which is low
stress(<300MPa) and Particle-free. I have search a lot of papers on internet
.. The only way to get low stress Si3N4 is increasing DCS/NH3 ratio , but
particle contamination is getting worse. Is there anyone can share
informations about how to deposite low stress Si3N4 in LPCVD without
particle contamination.

Thanks in advance.
Wang


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Tanner EDA by Mentor Graphics