MEMSnet Home: MEMS-Talk: Meaurement of noise characteristics of microbolometers
Meaurement of noise characteristics of microbolometers
2007-03-07
D. Zhou
2007-03-07
Wilson, Thomas
Meaurement of noise characteristics of microbolometers
Wilson, Thomas
2007-03-07
Dear Da-xiang:

The best paper I've come across regarding the computation and
measurement of noise in microbolometers (fore current and not
voltage-biased microbolometers) is "Apparatus for the study of the IR
multiple-photon resonances of polyatomic molecules via th eoptothermal
technique. II. The superconducting bolometer", in Rev. Sci. Instrum, 61
(5) pp. 1379-1389 (1990).

Good luck. Let me know if you find other good ones.

Thomas

Thomas E. Wilson
Professor of Physics
Marshall University
Science 154
One John Marshall Drive
Huntington, WV  25755-2570

Tel: 304.696.2752
FAX: 304.696.3243

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation