PDMS Alignment stage
Brian C
2007-05-02
EV Group produced a limited number of Contract Aligner EVG620's with
additional engineered microcontact printing, and nanoimprint lithography
capability. We purchased one in 2004 and have utilized this capability to
align objects such as PDMS to glass, etc. It has refined optics, and
mechanics to allow for thicker, and off-size substrates.  For more
information or questions contact me.  Brian Czimback, Cleanroom Operations,
Nanobiotechnology Center, Cornell University, Ithaca, NY. Email is
[email protected].


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.