Au electroplating
2007-05-09
kris
2007-05-09
David Nemeth
2007-05-10
Shay Kaplan
2007-05-10
P.E.M. Kuijpers
2007-05-10
David Nemeth
2007-05-10
David Roberts
2007-05-11
P.E.M. Kuijpers
2007-05-11
David Roberts
2007-05-14
P.E.M. Kuijpers
Miniature Hot Press for Plastic Microdevice bonding
2007-05-14
Heiko van der Linden
2007-05-14
David Roberts
2007-05-14
Mo Kebaili
Au electroplating
P.E.M. Kuijpers
2007-05-11
Hello Dave,

Another question about wafer plating:
We did install ENIG (Eletroless Nickel/Immersion Gold, Rohm and Haas
chemicals).
After Nickel plating we observed outplating of our Ni bath? We do have N2
bubbling in our bath for extra agitation.
Is there another simple solution to avoid this outplating?

Thanks in advance,
Peter Kuijpers
MiPlaza
DTS/TFF
High Tech Campus 04
Room: WAGp5-11
5656 AE Eindhoven
The Netherlands

Phone.:  (+31 40 27) 98904 (mobex)
mobile:(+31) 06-12507027
fax.:     [+31 40 27) 44769
mailto:[email protected]


"David Roberts"  writes:
Subject RE: [mems-talk] Au electroplating Classification

Hi Peter,
Cathodic activation at 20mA/cm2 in 10%sulfuric. Keep wet. Plate gold.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Nano-Master, Inc.