This is a multi-part message in MIME format.

--------------7DC03E954DAC
Content-Type: text/plain; charset=us-ascii
Content-Transfer-Encoding: 7bit

RobPearce1 wrote:
>
> I believe I have an application for MEMS technology in one of my current
> design projects. However, I know very little about the subject. Can anyone
> recommend an introductory text or design guide. The design requires a
> microvalve for use with high temperature gasses.

Redwood engages in the design and manufacture of microvalves whose
actuation principles are based on thermopneumatic expansion of a silicon
membrane.  I am attaching a paper which discusses some of the design
aspects of these valves.  Please cite as appropriate.  Note that
Redwood, and others, have valves designed for higher temperatures (how
high?), which are protected by patent.

The attached file is an Adobe PDF file.

Al
--
Albert K. Henning, Ph.D.    650/617-0854 (Office)
Redwood Microsystems        650/326-9217 (FAX)
1020 Hamilton Avenue        [email protected]
Menlo Park, CA  94025       http://www.redwoodmicro.com



 isis97.pdf


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.