XeF2 etch on W
2007-05-24
kris
2007-05-24
Bill Flounders
2007-05-24
Kirt Williams
XeF2 etch on W
Bill Flounders
2007-05-24
Yes. Rapidly

kris wrote:
> Hello,
>
> I am using XACTIX to etch Si. I have Tungsten layer on
> silicon. I was wondering if XeF2 etches Tungsten.
reply