Dear Alls
    I wonder if anybody have the experience of making Cr mask by dry etching. We
are drawing the pattern by EB on the ebr9 EB resist by it seems that it doesn't
work well in dry etching with cl2 and o2. The resist is ripped off. Can anyone
give us some suggestion about the resist and etching gas
    Thank you so much
               paynee



---------------------------------
Start Yahoo! Auction now! Check out the cool campaign
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
The Branford Group