Dear All,

I am trying to pattern a 15 micron wide channel in 15 micron thick SU-8 10.
My substrate is a 1 mm thick piece of Sapphire with 100 Ang. Ti/500 Ang. Au
atop.  I can't seem to get the channel to come out.  If I use longer
exposure times, it looks like I've overexposed and the channels don't
develop. However, as I use shorter exposure times, my channel edges become
more and more rough.  I believe it is because the Au on Sapphire is
reflecting more and causing the SU-8 to partially expose where it shouldn't
be.  I'm not sure though.  Any ideas on how to get the channel to develop
with clean lines?

Thanks,
Dan
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Addison Engineering
Process Variations in Microsystems Manufacturing