How to remove polymer on the sidewall after DRIE?
G Gan
2007-06-25
I am trying to find a process (prefer plasma) to remove the residual polymer
on the side-wall after DRIE etch (Bosch process). I am sure some people have
done this before, can you let me know the process (O2 plasma or other?) Btw,
how can you measure the residual polymer thickness before and after
stripping process? Thanks!

Gene
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.