Hi

The clean room class depends on how small will be your structures,
only for don't block your channels with dust or every else. I make
fluidical channels about 50mu only under a simple laminar flow.( [8^)
!!!)

About the quantity of free monomers, you can clean your linked PDMS
with organic solvents ( like acetonitrile or even acetone or
isopropanol ) to get rid of then. If you want, drop me a line and I
can search an article I've seen on eliminating free monomers from
PDMS.

Good Luck!!!

NH


> Betreff: [mems-talk] polymer fabrication
>
> Hellos all, I have some questions if there is one ho need to help me!
> - i need to have some informations for polymer fabrciation (especially
> using PDMS ),  and if there is contaminations problems with CMOS process?
> - what the clean room class if we need to fabricate bio-chip (or
> microfluidic devices)?
> Thanks
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
The Branford Group
Tanner EDA by Mentor Graphics