MEMSnet Home: MEMS-Talk: Si diphragm
Si diphragm
2007-08-10
ashwini jambhalikar
2007-08-10
Bill Flounders
Si diphragm
ashwini jambhalikar
2007-08-10
Dear Friends,

While making 20 micron -40 micron diaphragm in DRIE machine, I have observed
that the diaphragm gets popped up from the non exposed side.(the side which
is not seeing plasma).
Has anybody encountered something similar..what can be the possible cause of
this..has anybody encountered similar behaviour in wet etching..

Thanks,
Ashwini.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing