Hello All,

I was wondering if we can get a continuous thin metal
film (sputtering or evaporation)on the top of the
silicon wafer that is subjected to DRIE in STS system.


The released DRIE`d structures should be conductive
for the actuation with the adjacent substrate.

Thanks,
Kris