MEMSnet Home: MEMS-Talk: Difficulties with finding the alignment markings duringthe photolithography on ceramic substrates
Difficulties with finding the alignment markings during the photolithography on ceramic substrates
2007-11-12
Denis Petrov
Difficulties with finding the alignment markings duringthe photolithography on ceramic substrates
2007-11-12
Bob Henderson
Difficulties with finding the alignment markings duringthe photolithography on ceramic substrates
Bob Henderson
2007-11-12
Make you first alignment on a film like nitride or aluminum that will show
thru subsequent layers. Bob Henderson
----- Original Message -----
From: "Denis Petrov" 
To: 
Sent: Monday, November 12, 2007 8:08 AM
Subject: [mems-talk] Difficulties with finding the alignment markings
duringthe photolithography on ceramic substrates


Hello,

I have several ceramic wafers to be exposed. While trying to complete
the subsequent photolithography steps, I have encountered the
following problem.
Due to the roughtness of the ceramic surface, it is very difficult to
recognize the alignment marks (or even the structure patterns) in the
microscope... As a consequence, misalignments occure, and that spoils
all the previous work.
Does someone know how to overcome this, or how to enchance the
visibility of the markings?

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Tanner EDA by Mentor Graphics