Etching silicon nitride
2008-01-08
Sandip Agarwal
2008-01-08
Bill Moffat
2008-01-08
Edward Sebesta
2008-01-08
Bob Henderson
2008-01-09
Kvel Bergtatt
Etching silicon nitride
Sandip Agarwal
2008-01-08
I want to pattern silicon nitride by etching with hot phosphoric acid.
What are the photoresists that would withstand these etching conditions?


Sandip Agarwal

Senior Scientist
Nano-Terra Inc.
790 Memorial Drive, Suite 202
Cambridge MA 02139
0 617 621 8500 x2302   C 713 471 0916   F 617 621 8501
[email protected] 
www.nanoterra.com 

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Nano-Master, Inc.
Harrick Plasma, Inc.