MEMSnet Home: MEMS-Talk: Fracture strength for Au Cantilever.
Fracture strength for Au Cantilever.
1998-08-21
N K Choudhary (97307404)
Fracture strength for Au Cantilever.
N K Choudhary (97307404)
1998-08-21
Hello,
      I would appreciate if someone could provide me with information on
determining the shear strength for sputtered & then electroplated Cr+Au.(
500 A Cr and 5 um Au ).
        How will the shear strength wil change as a function of
cantilever dimensions ( length + width + thickness).

Thanking you all in advance
Regards
NKC


******************************************************************************
Sqr Ldr N K Choudhary                         Residential Address.
M.Tech (II).Electrical Engg.                  Flat No 304, DRDO Bldg
Microelectronics.                             IIT POWAI
IIT Powai.
Bombay- 400 076.
Tel:  578 3655                                Bombay- 400 076.
email:  
******************************************************************************


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
The Branford Group