A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Titanium etch
Titanium etch
2008-03-07
Michael Cooke
2008-03-07
Brent Garber
2008-03-08
Deepasree Konduparthi
Titanium etch
Deepasree Konduparthi
2008-03-08
TFTN is a HCl based etchant from transene

On Fri, Mar 7, 2008 at 12:39 PM, Brent Garber  wrote:
> Mike,
>
>  H2O2 @ 50c
>
>  Brent
>
>
>  Michael Cooke wrote:
>  > Dear all,
>  >
>  > I was wondering if there is a safer etch for Titanium which I haven't
>  > come across which doesn't involve HF or HF as a biproduct. Ideally it
>  > should be done at room temp.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
The Branford Group
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.