MEMSnet Home: MEMS-Talk: Hydrophobic treatments/coatings for Polycarbonate
Hydrophobic treatments/coatings for Polycarbonate
2008-04-09
Paul Monaghan
2008-04-09
Adrian Brozell
2008-04-09
Paul Monaghan
2008-04-09
Boris Kobrin
2008-04-10
Paul Monaghan
Hydrophobic treatments/coatings for Polycarbonate
Paul Monaghan
2008-04-09
Adrian,

You are correct that plasma oxidation will increase the hydrophilicity of
the surface. My understanding is this should also generate carboxylic acid
(COOH) or other functional groups, hence the decrease in contact angle.
This may offer a route to chemically modifying the surface such as using a
carbodiimide chemistry etc. This is why I mentioned plasma oxidation.

Yes, PC is relatively hydrophobic but I would like to make it more so.

Best regards,

Paul

Quoting Adrian Brozell :

> Oxidation makes it hydrophilic.  Polycarbonate should be reasonably
> hydrophobic like most plastics.
>
> adrian
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics