su8 1000um thick
Jian Wang
2008-04-14
Dr. Amit Asthana of Chungnam National University supplied an unpublished
protocol in this forum around last September. The method worked for making 1
mm thick SU8. You can search the list.

Jian Wang
Senior Staff Scientist

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Abhishek Jain
Sent: Sunday, April 13, 2008 12:28 PM
To: General MEMS discussion
Subject: [mems-talk] su8 1000um thick

Dear forum members

I want to make 1mm thick structures on SU8 for doing soft lithography with
PDMS later on. It is only one mask and just straight channels.

I have SU8 2075 with me and I am trying to find a recipe for doing this. If
anyone has experience in dealing with this, I will truly appreciate if you
may give some insight on the method...

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Nano-Master, Inc.
Addison Engineering