A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Gold evaporation coating on silicon.
Gold evaporation coating on silicon.
2008-05-01
Moshe
2008-05-01
Andrea Mazzolari
2008-05-01
Shay Kaplan
2008-05-01
Roger Shile
2008-05-01
Roger Shile
2008-05-01
Kevin Paul Nichols
Gold evaporation coating on silicon.
Kevin Paul Nichols
2008-05-01
Moshe,

In addition to Cr (as mentioned in other emails), Ta and Ti also work as
adhesion layers for Au on Si.

Kevin Paul Nichols
MESA+ Institute for Nanotechnology
Mesoscale Chemical Systems
Meander 151
University of Twente
Postbus 217
7500 AE Enschede
The Netherlands

Office: +31 (0)53 489 26 31
Mobile: +31 (0)6 49 312 471
Fax   : +31 (0)53 489 35 95
Email : [email protected]
Web   : http://mcs.tnw.utwente.nl/


> From: Moshe 
> Reply-To: General MEMS discussion 
> Date: Wed, 30 Apr 2008 22:14:14 -0700 (PDT)
> To: 
> Subject: [mems-talk] Gold evaporation coating on silicon.
>
> Hello
>
> I want to coat silicon with evaporation coating, and
> to assurance that the adhesion between the two
> materials  will be optimal.
> What will be  the optimal treatment to achieve
> adhesion ?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
MEMStaff Inc.
Process Variations in Microsystems Manufacturing