I have tried to make 5um thick PR as sacrificial layer.
But big shrinkage & roughness occured baking smaple in conventional
oven for another layer deposition. So, we tried anthor baking method
,UV curing. we had good enough results of smoothness, which is not
the best,I think. The better condition or perfect smoothness should
be challenged.

Dose anyone give me recommendation for better results ?


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Mentor Graphics Corporation
Addison Engineering