A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: 20um features using AZP4620
20um features using AZP4620
2008-06-03
Haixin Zhu
2008-06-04
李加东
2008-06-04
Haixin Zhu
2008-06-04
Robert Black
2008-06-04
Haixin Zhu
2008-06-13
Brubaker Chad
2008-06-13
Haixin Zhu
2008-06-15
Tolga YELBOGA
2008-06-16
Oakes Garrett
2008-06-04
Tolga YELBOGA
2008-06-04
Haixin Zhu
20um features using AZP4620
Haixin Zhu
2008-06-03
Dear all,

I am trying to produce 20um features using AZP4620, the thickness is
required to be 38um, I tried double coating/triple coating with various
spin speed and baking condition, and they did not work. Is there any one
having this experience and advise me on the right direction?

Appreciate the help

Michael

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing