BCB cure
2008-06-27
Cassie Iany
2008-06-27
P.E.M. Kuijpers
2008-06-29
Cassie Iany
2008-06-30
Trent Huang
BCB cure
Cassie Iany
2008-06-29
The thickness is about 20 um. The ramp up speed is about 2 degree per minute.
Basically I follow the guidline given by supplier.