MEMSnet Home: MEMS-Talk: Ni plating on Au film
Ni plating on Au film
2008-07-16
Qi Luo
2008-07-18
汪飞
2008-07-20
Moshe
2008-08-06
Petru Lunca Popa
Ni plating on Au film
Petru Lunca Popa
2008-08-06
Hi
I am also plating Ni on Au using a Ni sulfamate solution
CAn you please tell me more detrails about you Ni plating proicess?
What solution you use?  What plating potentials?

On Sun, Jul 20, 2008 at 11:07 AM, Moshe  wrote:
> Nickel strike is a thin  intermediate film that made from 210 gr/ liter Nickel
Chloride , 90ml/liter HCl - and the rest is DI water .
> This  intermediate make the adhesion bettwen the metal and the Nickel.
> It usually use to make adhesion between stainless steel and Nickel.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
Process Variations in Microsystems Manufacturing
The Branford Group