Commercial Vendors of Silicone membranes
2008-08-20
Nano world
2008-08-21
Brian Stahl
2008-08-22
Le Cao Hoai Nam
2008-08-22
[email protected]
2008-08-23
Le Cao Hoai Nam
2008-08-23
Matthew Davies
2008-08-24
Barbara Cortese
Commercial Vendors of Silicone membranes
Le Cao Hoai Nam
2008-08-23
Hi Seyed,

I am sorry. I haven't tried such thin PDMS membranes. However, you may
try to increase the spin speed and time to see if you can achieve
that. Note that you should pour PDMS equally everywhere on the
substrate to enhance the membrane thickness's uniformity.

Greetings,
Nam Le
Ritsumeikan University, Japan

On Sat, Aug 23, 2008 at 1:12 AM,   wrote:
> Hi,
> Wonderful, I am trying to spin aroud 10 micrometer of Sylgard 184 on 1 to 2
> inch
> glass wafers. Could you please tell me the spin parameters required to do
> such a thin layer of PDMS.
> I appreciate yoy comments.
> Thank you
>
> Seyed
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
University Wafer
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing