Thermal bonding problem
2008-09-02
Lin Yu
2008-09-03
Balaji
2008-09-03
Lin Yu
2008-09-04
Balaji
2008-09-03
Brad Johnson
Thermal bonding problem
Balaji
2008-09-04
Hi Lin

I dont think the soft material might help in reducing the shear force.

Balaji
----

On Wed, Sep 3, 2008 at 10:27 PM, Lin Yu  wrote:

> Hi Balaji,
>
> Thanks. Do you think if applying some soft material on the substrates of
> both
> samples can help in this case?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Addison Engineering
Mentor Graphics Corporation