MEMSnet Home: MEMS-Talk: grinding/polishing equipment suggestion
grinding/polishing equipment suggestion
2008-09-20
Andrea Mazzolari
grinding/polishing equipment suggestion
Andrea Mazzolari
2008-09-20
Good morning everyone.

We are interested in equipment for grinding/polishing.
-We need to produce wafers as thin as 50um
-We need to produce wafers with TTV<1 and and preferably, flatness less
than about 300nm over an area of 30x10 mm
-We don't need fully automated equipment, cos this tool will be used for
R&D purposes.
-We can accept to buy used and refurbished equipment

I'm looking for suggestions about possible brands and sellers of this kind
of equipment.

Many thanks,
Andrea


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
University Wafer
The Branford Group