2008-10-09
Hi,

You can try RIE dry etch prosess in a ambient of CCl2F2 (Freon-12) gas for dry
etching of GaN.
This prosess is suitable for AlGaN dry etch also. Etching rate changes with Al
content of structure.

Best Regards.