MEMSnet Home: MEMS-Talk: PEG-coating of sealed glass or silicon channel?
PEG-coating of sealed glass or silicon channel?
2008-11-14
Mikael Evander
2008-11-14
Bill Moffat
PEG-coating of sealed glass or silicon channel?
Mikael Evander
2008-11-14
Hi.

Does anyone know of a good protocol or reference for coating a sealed
glass or silicon channel with PEG (or something similar)? I'm trying to
reduce the amount of sticking of particles/cells to the surfaces and was
told that PEG might do the trick?

best regards

Mikael Evander                      Tel:   +46-46-222 75 27
Lund University                     Mobil: +46-702 27 11 58
Dept. of Electrical Measurements    Fax:   +46-46-222 45 27
Box 118
221 00 Lund
Sweden
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
MEMS Technology Review
Process Variations in Microsystems Manufacturing