A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Stress reduction in SOI
Stress reduction in SOI
2008-12-15
Jason Milne
2008-12-15
Andrea Mazzolari
2008-12-16
Jason Milne
2008-12-15
Michael
2008-12-16
[email protected]
2008-12-19
Trent Huang
Stress reduction in SOI
Michael
2008-12-15
Hi Jason

Do you have any oxide layer on your micro-bridge or cantilever devices?
Are they a single layer structures? It is important that you are sure you made
the structures out of the device layer only.
regards,





________________________________
From: Jason Milne 
To: General MEMS discussion 
Sent: Monday, 15 December, 2008 5:10:28 PM
Subject: [mems-talk] Stress reduction in SOI

Hi mems-talk,

I purchased some thin SOI recently to make some fixed-fixed beams and
cantilevers, and I was assuming that the device layer would be close to
zero stress (slightly tensile, if anything) and have no stress
gradients. Having made the structures, it seems that the device layer is
compressively stressed (the fixed-fixed beams buckle) and has a stress
gradient (the cantilevers curl upwards). I was wondering if anyone has
tried to anneal SOI wafers to reduce stress and/or stress gradients, and
if so, what conditions did you use?

The SOI has a 260nm thick device layer and 2000nm thick oxide layer, if
that helps.

Regards
Jason Milne
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Harrick Plasma, Inc.