MEMSnet Home: MEMS-Talk: Dry etch of AlGaAs over InGaP and GaAs
Dry etch of AlGaAs over InGaP and GaAs
2009-01-13
Zhaoyu Zhang
2009-01-14
Kumar, Parshant
Dry etch of AlGaAs over InGaP and GaAs
Zhaoyu Zhang
2009-01-13
Dear Mems-talk,

I am wondering if any gas could be used to etch Al0.8GaAs over InGaP and GaAs
(etch AlGaAs with InGaP and GaAs intact)? I have both RIE and ICPRIE system for
this dry etch. I prefer isotropic etching.

Bests,
ZZ