MEMSnet Home: MEMS-Talk: Deposition of Chromium and Platinum
Deposition of Chromium and Platinum
2009-01-19
Yinyan Gong
2009-01-19
Ruiz, Marcos Daniel (SENCOE)
2009-01-20
Yinyan Gong
2009-01-20
Ruiz, Marcos Daniel (SENCOE)
2009-01-19
John Hilton
2009-01-19
Edward Sebesta
2009-01-20
Yinyan Gong
2009-01-20
Edward Sebesta
2009-01-22
Evelyn B
2009-01-20
Jie Zou
Deposition of Chromium and Platinum
Yinyan Gong
2009-01-20
Substrate is boron compound and the total thickness of the metal layer
is 150nm. The thickness of Shipley 1165 is about 1.3um.

Yinyan

Ruiz, Marcos Daniel (SENCOE) wrote:
> What substrate material are you using?  How thick are the metal layers?
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics