MEMSnet Home: MEMS-Talk: Double lithography problem with SU1828-TI35ES
Double lithography problem with SU1828-TI35ES
2009-01-29
basar bolukbas
2009-01-29
Bill Moffat
2009-01-30
basar bolukbas
2009-01-30
Bill Moffat
2009-01-30
basar bolukbas
2009-01-30
Edward Sebesta
2009-01-30
basar bolukbas
2009-02-02
Edward Sebesta
Double lithography problem with SU1828-TI35ES
Bill Moffat
2009-01-29
Yes you need to Silylate the first resist.  The Silicon barrier you set
up will stop the second resist solvent dissolving the first resist.

Bill Moffat

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of basar bolukbas
Sent: Thursday, January 29, 2009 10:36 AM
To: [email protected]
Subject: [mems-talk] Double lithography problem with SU1828-TI35ES

Hello everyone,

I am making lithography with SU1828. After patterning of this resist, i
need to make a another lithography on top of SU1828's patterns, but when
i spin to other resist (TI35ES) the solvent of TI35ES dissolves to
patterns of SU1828.

Do you have similar experience?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Mentor Graphics Corporation