A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Wet etch of Si
Wet etch of Si
2009-02-05
KUIJPERS, Peter
2009-02-05
Fei Wang
2009-02-05
Brian Stahl
2009-02-11
Kvel Bergtatt aka fmaya
Wet etch of Si
KUIJPERS, Peter
2009-02-05
Hi all,

Is there a recipe for wet anisotropic etching of Si?
Now we use KOH on {1,0,0} wafers, resulting in a slope of 54.7°.
Maybe another crystal orientation and/or etching agent.

Thanks in advance

Peter Kuijpers
MiPlaza Technology Laboratories
Philips Research Europe
reply