Dehydration bake
Yinyan Gong
2009-02-09
This will evaporate any moisture presenting on surface of a wafer and
thus promotes adhesion of photoresist.

Evelyn B wrote:
> I have seen dehydration bakes used as part of solvent cleaning of glass and
> sapphire substrates. What is the purpose/advantage of this bake?
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
The Branford Group
Process Variations in Microsystems Manufacturing