Yoshi, If you have Au/Ti then the Ti form a VERY stable oxide.  It is most
likely that NOT the Au that is oxidizing.  Au does not WANT to oxidize, Ti
does. Gary

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Gabriel Matus
Sent: Friday, March 13, 2009 2:12 PM
To: [email protected]
Subject: Re: [mems-talk] Gold Oxide


Yoshi,

Oxygen plasma can oxidize the surface of gold.  If that's what you have,
then 15 seconds in BOE or 30 seconds in an SF6 plasma will etch the oxide.

If that's not what you have, then you'll have to do XPS or some other
chemical analysis to try to identify it.

Gabriel
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMS Technology Review