A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Re: Micromoulding and joining
Re: Micromoulding and joining
1998-09-22
Hubert Lorenz
1998-09-30
[email protected]
1998-10-18
[email protected]
Re: Micromoulding and joining
[email protected]
1998-09-30
>      Chris Turner:
>
>      Hello,
>      Does anyone have any information on moulding (particularly
>      compression moulding) of micro-structures in polymers
>      (particularly polypropylene). Also is there any information out
>      there on joining of moulded parts to form microfluidic
>      structures. Any information, or pointers to sources of info,
>      gratefully received. Thank you.

Hello Chris,

I have no other information on moulding of micro-structures other
than that it may not be the right process for your purposes. Have you
heard about embossing yet? Here are the ones to ask, especially for
microfluidic structures (don't ask me):

Jenoptic Mikrotechnik
Prüssingstr. 41
07745 Jena
Germany

Manager:
Lutz Müller
Phone: (0)3641- 65 - 3182

Marketing (english speaking):
Hartmut Blum
Phone: (0)3641 - 65 - 3338

Fax:  (0)3641 - 65 - 3562

This is a recommendation from Mr. Dieter Stolze, who I asked about
the matter.

Sincerely yours,
Ralf Longwitz.


______________________________________

 CiS Institut fuer Mikrosensorik e.V.
 Haarbergstr. 61
 D - 99097 Erfurt

 e-mail: [email protected]
 tel:       0361 / 42051 - 15
 fax:      0361 / 42051 - 13

 http://www.cismst.com
______________________________________


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
University Wafer