MEMSnet Home: MEMS-Talk: SU8 shrinking
SU8 shrinking
2009-03-31
[email protected]
2009-03-31
Gareth Jenkins
2009-03-31
郑瑞麟(Ruilin Zheng)
2009-03-31
Ed
SU8 shrinking
[email protected]
2009-03-31
hi all
      i am spin coating SU8 2050 on piranha cleaned silicon wafer but
    during prebake it is shrinking and coming into the center of the
    wafer. What could be the possible cause ?
--
Kamlesh Pawar
M.Tech (Biomedical Engg)
Mob :+919870062960
IIT-Bombay