Greetings

To make vias-small holes in glass,there are basically 2 low cost options
micro particles blasting or diamond drilling
Diamond drilling is done at high speed 10000 rpm or so.
One may try an dremel tool however the run out can be a proplem .
We use an air driven motor the spindle for all practical purpose has no run out.
With a diamond drill it will take seconds to get 2 mm dia holes
With the micro particle scheme we use a mask and than blast.
Hope this gives you an idea what to expect.
Regards
[email protected]
Dov
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation