A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Anybody using Sb/Au or Sb/Ag contact before?
Anybody using Sb/Au or Sb/Ag contact before?
2009-06-10
Chong Liu
Anybody using Sb/Au or Sb/Ag contact before?
Chong Liu
2009-06-10
Hi,

Does anybody have some experience in using Sb/Au or Sb/Ag as contact for
n-type Si? I tried recently and I have some problem with the lift-off after
thermal evaporation of 10nm Sb and 100nm Ag. Is there anything reaction
happening here?

By the way, is this a good candidate for small contact area, like ~1um wide
electrode?

Thank you so much!

Chong
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Tanner EDA by Mentor Graphics
MEMS Technology Review
Process Variations in Microsystems Manufacturing