Hi everybody,

I need to deposit P3HT (a conducting polymer) from disolution in a 10cmx10cm
substrate, and I need to control de thickness of the layer around 100-200nm. We
used to make it by spincoating with smaller substrates, now I would like to test
other techniques (doctor blade, inkjet printing...)., but I dont know if it is
possible with such thin layers.  Any suggestions?

Also, for the spincoating we used toluene for the solution, but with continuous
processes, should we change the solvent to another one with more viscosity?

Thank you very much in advance.

Rafael García Valverde
Dept. Electrónica, Tecnología de Computadores y Proyectos (ETSIT)
Electronics, Computer Technology and Projects.
Technical University of Cartagena (UPCT)
Tlf: (+34) 868-888787
Addr: Plaza del Hospital,1 30202 Cartagena (Murcia) SPAIN
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
The Branford Group
University Wafer