MEMSnet Home: MEMS-Talk: silicon etching with KOH solution 10%
silicon etching with KOH solution 10%
2009-10-28
Jing Xiao
2009-10-29
Shao Guocheng
2009-10-29
Fei Wang
2009-10-29
Nathan McCorkle
2009-10-30
Brian Stahl
silicon etching with KOH solution 10%
Brian Stahl
2009-10-30
BOE etches oxide, KOH etches silicon.  BOE etching of oxide is isotropic,
KOH etching of silicon is anisotropic.  Surface quality depends entirely on
etching parameters (concentration, temperature, agitation, surfactants,
etc.).  I would imagine that BOE surface quality is more dependent on the
surface quality of the silicon beneath the oxide than of the oxide itself...

--
Brian C. Stahl
Graduate Student Researcher
UCSB Materials Research Laboratory
[email protected] / [email protected]
Cell: (805) 748-5839
Office: MRL 3117A


On Thu, Oct 29, 2009 at 10:28 AM, Nathan McCorkle  wrote:

> How does KOH compare to BOE in surface quality? Is one more or less
> isotropic?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.